Sub-Critical Annealing

Many stampings that under go deep draws and severe forming operations exhibit high cold work hardnesses that prevent further drawing or stamping operations.  Sub-critical annealing is an ideal way to remove these stresses to allow subsequent forming operations.  The temperature ranges for this process typically range from 1250F to 1400F.